Investment Castings problem -- surface defects caused by ...?

by Paul Wilson <pwilson@[EMAIL PROTECTED] > Apr 7, 2008 at 07:17 PM

Folks,
I sent some very nice waxes off to be cast in sterling, but a few came
back with surface defects.   My casting guy says it's because the cast
pieces were "too heavy."   I think it was a problem with the investing
technique.

What is your diagnosis?  I posted pictures at
www.eliasbing.com/surface_defects.html.


Thanks,
Paul
 




 7 Posts in Topic:
Investment Castings problem -- surface defects caused by ...?
Paul Wilson <pwilson@[  2008-04-07 19:17:11 
Re: Investment Castings problem -- surface defects caused by ...
"Peter W.. Rowe,&quo  2008-04-07 19:43:33 
Re: Investment Castings problem -- surface defects caused by ...
Paul Wilson <pwilson@[  2008-04-09 18:26:01 
Re: Investment Castings problem -- surface defects caused by ...
"Peter W.. Rowe,&quo  2008-04-09 18:49:07 
Re: Investment Castings problem -- surface defects caused by ...
Heinrich Butschal <deb  2008-04-08 09:40:27 
Re: Investment Castings problem -- surface defects caused by ...
"Séimí mac Liam"  2008-04-18 08:38:56 
Re: Investment Castings problem -- surface defects caused by ...
Heinrich Butschal <deb  2008-04-20 11:01:09 